Results of Non-Destructive and Destructive Tests of Welded Joints Made of Heat-Resistant Cast Steel GX40NiCrSiNb35-25 in Welding Procedure Qualification

Sławomir Parzych
Keywords: 
GX40NiCrSiNb35-25, heat-resistant cast steel, welding procedure qualification, destructive tests
doi: 
10.17729/ebis.2017.2/4